Impression creep test of a P91 steel: a round robin programme

Research paper by S. J. Brett, C. N. C. Dyson, D. Purdy, J. Shingledecker, J. Rantala, J. Eaton-Mckay, W. Sun

Indexed on: 07 Mar '18Published on: 14 Dec '17Published in: Materials at High Temperatures



Abstract

Authors: S. J. Brett, C. N. C. Dyson, D. Purdy, J. Shingledecker, J. Rantala, J. Eaton-Mckay, W. Sun Article URL: http://www.tandfonline.com/doi/full/10.1080/09603409.2017.1410330?af=R Citation: Materials at High Temperatures Publication Date: 2017-12-14T07:16:07Z Journal: Materials at High Temperatures